简体中文
埋弧焊丝 埋弧焊丝

SW-EB3

Hits:78

EB3

SUBMERGED ARC WELDING WIRE: SW-EB3


Specification:AWS  A5.23   EB3

                        ASME/SFA 5.23  EB3

                        ISO 24598-A-S SCrMo2

                        ISO 24598-B SU2C1M

                        GB/T 12470 SU2C1M


Introduction:

  1. For 620Mpa grade 2.25%Cr-1%Mo heat-resisting steel.

  2. Well weldability: stable arc, easy slag removal,neat weld bead.


Application:

  1. Thermal power plant

  2. Petroleum refinery


Pass the certification:

Contact us


Chemical Composition of Wire %:


CMnSiPSCuCrMo
AWS0.05-0.150.40-0.800.05-0.30≤0.025≤0.025≤0.352.25-3.000.90-1.10
TR(HC)0.090.620.100.0110.0030.112.600.99


Mechanical Properties of Deposited Metal:


Tensile StrengthYield StrengthElongationImpact Value
MpaMpa%20℃    J
TR(HC)57048025150


Diameter/Packing:

DiameterHollow CoilDrumSpoolBasket
mm/in25kg(55lbs)50kg(110lbs)60Kg(132lbs)100Kg(220lbs)150Kg(330lbs)250Kg(550lbs)350Kg(770lbs)250Kg(550lbs)350Kg(770lbs)20Kg(44lbs)25kg(55lbs)
1.0(0.040)








1.2(0.045)








1.4(0.052)








1.6(1/16)




2.0(5/64)







2.4(3/32)


3.0(0.118)


3.2(1/8)


4.0(5/32)


4.8(3/16)


5.0(0.197)


6.0(15/64)






6.4(1/14)







Welding position:PA


  1. Points for Attention:

    1. The Welding flux must be baked under 350-400℃  for 2~4 hours.

    2. Remove the oil, dust and rust from the welding parts



Previous:SW-EB2

Next:SW-EM2
Related Products

Online message

Name

Tel

Content

Contact us

Zhangjiagang HengChang Welding Materials Co.,Ltd.
© 2024 Zhangjiagang HengChang Welding Materials Co.,Ltd.
技术支持: 云标科技